MEMSnet Home: MEMS-Talk: Does BOE solution disolve Ti/Al/Ti/Au?
Does BOE solution disolve Ti/Al/Ti/Au?
2010-05-24
QAZI, MUHAMMAD
2010-05-24
Anıl Günay Demirkol
2010-05-24
Harsh Sundani
2010-05-26
Pothisorn, Araya - potay006
2010-05-25
Li. Zhang
2010-05-25
Tony Price
Does BOE solution disolve Ti/Al/Ti/Au?
QAZI, MUHAMMAD
2010-05-24
Dear all,

Sample: AlGaN/GaN (2um) on Silicon substrate (500um)
Size: 1.4cmx1.4cm pieces

At some point of my process line I have Ti/Al/Ti/Au contact on the top side.
After that, I had to deposit PECVD 12um oxide on the back side to have pockets
for Si etch (SiO2 acts as masking layer for anisotrpic Si etch- Bosch process).
After I dip it in BOE soltion, the top contacts wash away :( .

Any solution or suggestion?

Muhammad Qazi
Dept of EE
University of South Carolina
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.