MEMSnet Home: MEMS-Talk: SiO2 under-etch
SiO2 under-etch
2010-05-29
priyesh dhandharia
2010-05-29
Prasanna Srinivasan
2010-05-30
priyesh dhandharia
2010-05-31
[email protected]
SiO2 under-etch
[email protected]
2010-05-31
Did I understand that SiC was deposited on the SiO2?

One potential cause is that the deposition of SiC reduced the SiO2 layer at the
surface, making it unetchable by flourides. I don't know what the etch rate of
SiO would be, but I suspect it would be slow.

With HF or BOE you should get some etch of the SiO2 even with 1 um contacts.
Especially with BOE, it is always sold as "super wet" or some such thing full of
surfactants.

Also, how would you be absolutely sure that you completely etched off the SiC?

Just some thoughts.

Ed


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer