MEMSnet Home: MEMS-Talk: Does XeF2 (Si isotropic etch) attack AlGaN-GaN?
Does XeF2 (Si isotropic etch) attack AlGaN-GaN?
2010-06-16
QAZI, MUHAMMAD
2010-06-17
David Springer
Does XeF2 (Si isotropic etch) attack AlGaN-GaN?
QAZI, MUHAMMAD
2010-06-16
Sample: 2.2um AlGaN-GaN on 500um Si substrate.
Process steps done: In selected areas AlGaN-GaN is etched down to Si.
Target: Etch Si further down.

I don't use RIE for Si etch, because I suspect the physical bombardment of
plasma may
damage the top 17nm AlGaN.

Possible solution:  XeF2 isotropic Si etch because its only chemical process
without any RF

QUESTION: Does XeF2 attack AlGaN-GaN ?


Muhammad Qazi
Dept. of EE
University of South Carolina
Columbia, SC29208
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.