MEMSnet Home: MEMS-Talk: Plasma activation of Magnesium Fluoride coated surfaces
Plasma activation of Magnesium Fluoride coated surfaces
2010-06-28
Danny Gossett
2010-06-29
Felix Lu
2010-06-29
Danny Gossett
2010-06-30
Felix Lu
Plasma activation of Magnesium Fluoride coated surfaces
Danny Gossett
2010-06-28
Dear Colleagues,

I'm attempting to bond a polydimethysiloxane (PDMS) block to an
antireflective coated window (Magnesium Fluoride, MIL-C-675). While
plasma activation of uncoated glass and PDMS followed by contact of
the two surfaces creates a strong covalent bond, the plasma does not
appear to activate the AR coated window in a way that allows the same
linkage. Does anyone have any suggestions as to how I might bond these
surfaces? Thank you so much.

Daniel Gossett
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group