MEMSnet Home: MEMS-Talk: Re: electroplating bath
Re: electroplating bath
1998-10-27
Kai Hiltmann
1998-10-26
Rajeshuni Ramesham
1998-10-26
Rajeshuni Ramesham
1998-10-26
Rajeshuni Ramesham
1998-10-27
Jong In Song
1998-10-27
Shekhar Bhansali
1998-10-27
Winston Chan
Re: electroplating bath
Winston Chan
1998-10-27
Cha-Mei Tang wrote:

> Does any one know electroplating suppliers that sells small or modest
> quantities of electroplating bath for research purposes?

It depends on what you are plating.  A company that sells a wide variety
of plating solutions is Technic (http://www.technic.com).  Another that
sells solutions aimed at electronics applications is Transene in Rowley,
MA.  I do not have a current phone number for them.

Winston Chan
--
Winston Chan                            | phone: (319) 353-2398
Dept. of Electrical Engineering         | fax: (319) 353-1115
University of Iowa                      | email: [email protected]
Iowa City, IA 52242


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.