Hi all,

I've tried to use PECVD oxide as etch mask in 74% phosphoric acid heated
at 130 deg, but it did not work.

In my understanding, silicon oxide should be resistant to phosphoric acid.

So what's wrong ?

Best regards,
Andrea
reply