A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Copper electroplating and Dry film resist
Copper electroplating and Dry film resist
2010-08-09
Sandeep Makhar
2010-08-10
Yingnan Wang
2010-08-10
Denis Petrov
2010-08-10
wangningyuan
2010-08-10
Ying-Tao Tian
2010-08-10
Sandeep Makhar
2010-08-10
Denis Petrov
Copper electroplating and Dry film resist
Ying-Tao Tian
2010-08-10
Hi Sandeep,

There are several possible reasons for your problem:

1. the non-plated area is still covered by the photoresist, you need to check
your photoresist after development.

2. your substrate pretreatment before photoresist patterning is not good enough
for electroplating.

3. if your pattern is very small, e.g. say less than 50 micron, you probably
need an additional pre-wetting step to make sure the pattern is completely
covered by the electrolyte.

Yingtao

________________________________________
From: [email protected] [mems-talk-
[email protected]] On Behalf Of Sandeep Makhar
[[email protected]]
Sent: 09 August 2010 20:13
To: [email protected]
Subject: [mems-talk] Copper electroplating and Dry film resist

Hello All-

We are pattern plating copper using a negative dry film photoresist. Post
plating we observe that there is some non-plated area between the dry film
and the plated area. It seems that this area is not wetted during the
plating operation. Does anyone know why this would happen? Thanking you.

Regards,
Sandeep
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation