MEMSnet Home: MEMS-Talk: KOH resistant paste
KOH resistant paste
2010-08-21
Temmuz
2010-08-23
Kuijpers, Peter
2010-08-24
roger brennan
2010-08-23
amit asthana
2010-08-24
Huy
2010-10-27
Wendell McCulley
2010-08-27
lamine nait
2010-08-28
Temmuz Ceyhan
KOH resistant paste
Kuijpers, Peter
2010-08-23
Hello all,

At our site we use LPCVD SiN or paryleen as protection for the frontside.


Peter Kuijpers
MiPlaza
Technology Laboratories
High Tech Campus 04
Room: WAGp5-11
5656 AE Eindhoven
The Netherlands
Phone.: (+31 40 27) 43667
mobile:(+31) 06-12507027
fax.: [+31 40 27) 44769
mailto:[email protected]
________________________________________
Van: [email protected] [mems-talk-
[email protected]] namens Temmuz
[[email protected]]
Verzonden: zondag 22 augustus 2010 1:14
Aan: [email protected]
Onderwerp: [mems-talk] KOH resistant paste

Hello,

I am trying to do back side etching to Si based SOI wafer entirely
(500um etch).  As etchant, I am using %30 KOH at 80 degrees for 7-8
hours.  In order to protect the topside, I am using 500nm thick nitride
layer, however, because of the void formations during PECVD SiN
deposition process, KOH etches everything on the topside.  DRIE is not
an option for me.  Finally I decided to paste my sample to glass in
order to etch only the backside.  Does anyone know of a paste, like
silver paste or epoxy, which can resist to extended hours of KOH etching
without getting etched at all?

OR!

Do anyone know of a way which I can protect the topside of my sample
during etching?

P.S.  As I read the archives, I learned that Protek B3 coating or
annealing to high temperatures (800 degrees) can work, however, as some
of the members say, coating is hard to remove and I can not anneal up to
800 or more degrees since my features include Al (it has melting point
of 660 degrees).

Thank you.

Temmuz CEYHAN
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing