Dear All,

I would realize patterned structures by selective etching of a nanometric
(10/20/30nm) gold layer deposited onto a titanium layer.

I read some protocols to etch chemically the gold but my question is how
selective is the process toward the gold rather than titanium?

Does anyone know companies that are able to deposit  and pattern in the metal
layer?

Thank you in advance.

Bests
Ed
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing