Hi all,

say you dip a  wafer in HF/BHF for a few seconds, pull it out,
rins with DI water and start your stopwatch (t=0). How quickly will
the native oxide layer grow at nominal conditions (room temp, 1 atm)?
How thick will it be after 1 day, 1 week, 1 year... etc?

Any info would be very interesting. Thanks a lot.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics