Porous Silicon recipe
2010-09-17
ANIRBAN SARKAR
2010-09-19
antwi nimo
Porous Silicon recipe
antwi nimo
2010-09-19
Anodization. But make sure the back side of your wafers is hightly doped to
ensure ohmic contact and the front side will have the pores.  The size of
the pores will of course depend on the current density, time, type of substrate,
illumination and so on.

Maybe this is the way to go.

nimo

________________________________
From: ANIRBAN SARKAR 
To: [email protected]
Sent: Fri, September 17, 2010 10:49:25 PM
Subject: [mems-talk] Porous Silicon recipe

Hello all,

I have been trying to generate porous silicon for our project but I am not
being able to obtain porous Silicon in the range of 50nm to 200nm.
I am requesting some insight in the recipe of generation of porous Si.

Any help will be gladly appreciated.

Thanks
Anirban
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review