RIE chamber cleaning
Zetao MA
2010-09-30
Hello,
   Our RIE 800 chamber cover is extremely dirty (for GaN etching), and we
soak it for a few days with Acetone. but the Acetone does not rinse the
coated materials at all. The Oxygen cleaning does not work either.
   Please give any advice to cleaning the Chamber cover, especially the
sidewall.

--
BR.
Dept. of EEE., CYC712,
University of Hong Kong.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
The Branford Group
MEMStaff Inc.