pyrex wafer thickness for anodic bonding
2010-10-14
Robert MacDonald
2010-10-14
Dr. Holger Becker
2010-10-15
Li zhuang
2010-10-14
Dean Hopkins
2010-10-15
Tony Rogers
pyrex wafer thickness for anodic bonding
Li zhuang
2010-10-15
Hi Rob, We've been working with pyrex about 1mm thick and sparingly about 1.
5mm, So what's your problem now?

Li Zhuang
University of Science and Technology of China

>Wondering if anyone has any experience anodic-bonding pyrex wafers to
>silicon wafers, where the pyrex is thicker than normal.

>For a 100mm wafer typical thicknesses I've worked
>with are in the 400-600um range. Has anyone had experience working with
>wafers 2 or 3 times thicker?

>Rob MacDonald
>Shearwater Scientific

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.