pyrex wafer thickness for anodic bonding
2010-10-14
Robert MacDonald
2010-10-14
Dr. Holger Becker
2010-10-15
Li zhuang
2010-10-14
Dean Hopkins
2010-10-15
Tony Rogers
pyrex wafer thickness for anodic bonding
Tony Rogers
2010-10-15
We have bonded to 10mm glass for an industrial yeast filter for beer!

________________________________

From: [email protected] on behalf of Dean Hopkins
Sent: Thu 10/14/2010 18:12
To: [email protected]
Subject: [mems-talk] pyrex wafer thickness for anodic bonding



Wondering if anyone has any experience anodic-bonding pyrex wafers to silicon
wafers, where the pyrex is thicker than normal.

For a 100mm wafer typical thicknesses I've worked with are in the 400-600um
range.
Has anyone had experience working with wafers 2 or 3 times thicker?

Rob MacDonald
Shearwater Scientific
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.