A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Etching a 1-2um slit through a Silicon wafer
Etching a 1-2um slit through a Silicon wafer
2010-10-21
Grimm, Dr. Daniel
2010-10-26
Nabhiraj Yalagoud
Etching a 1-2um slit through a Silicon wafer
Grimm, Dr. Daniel
2010-10-21
Hi guys,

I want to etch a slit (1-2um width at the top side, 200um long) through
a Si-wafer with 1um thermal oxide on top. I was thinking of a backside
etch selectively stopping at the SiO2, thus creating a membrane a little
bit larger than the final slit (I guess, control of the etch rates is
very challenging). Then, an additional dry etch of the 1-2um slit
through the oxide by RIE.

Do you know about a good process flow and/or do have any references?
Anything about a highly selective etchant, which mask (hard or soft) to
use, how to protect the front side etc.

Best wishes
Daniel

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group