copper plating
2010-10-26
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-28
Fei Wang
2010-10-28
Mingke Xiong
2010-10-27
Kuijpers, Peter
2010-10-27
Mingke Xiong
copper plating
Mingke Xiong
2010-10-27
Hi, Nabhiraj,

Yes, copper plating is much less expensive for mass production, so we want to
use silver as little as we can.

Mingke Xiong
AEM, Inc.
6670 Cobra Way
San Diego, CA 92121, USA
858-481-0210 ext. 1660
www.aem-usa.com

________________________________________
From: [email protected] [mems-talk-bounces+mxiong
[email protected]] On Behalf Of Nabhiraj Yalagoud
[[email protected]]
Sent: Wednesday, October 27, 2010 12:19 PM
To: General MEMS discussion
Subject: Re: [mems-talk] copper plating

Hello MIngke,

May i know your application? I am wondering why you are plating Cu on Silver? as
such Silver would do the job of Cu even in a better way. Or is it to reduce
the cost of mass production ?

Nabhiraj

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
University Wafer
Mentor Graphics Corporation