A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: copper plating
copper plating
2010-10-26
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-27
Nabhiraj Yalagoud
2010-10-27
Mingke Xiong
2010-10-28
Fei Wang
2010-10-28
Mingke Xiong
2010-10-27
Kuijpers, Peter
2010-10-27
Mingke Xiong
copper plating
Fei Wang
2010-10-28
Hi, Mingke,

You can try to combine your forward current pulse with a reverse cycle.

Best regards,
Fei

2010/10/27, Mingke Xiong :
> Hi, Nabhiraj,
>
> Yes, copper plating is much less expensive for mass production, so we want
> to use silver as little as we can.
>
> Mingke Xiong

--
Best regards,
Yours sincerely
Fei Wang
______________
Assistant Professor, Dr
MIC - Department of Micro and Nanotechnology
Technical University of Denmark (DTU)
Building 344, 1st floor, Room no. 130
DK-2800, Kgs. Lyngby
Denmark
Tel:  +45 4525 6311
Fax:  +45 4588 7762
Email: [email protected]
       http://www.nanotech.dtu.dk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing