Hi Rais,

I have only just seen your response (over a year later). I am interested
in diffusing lithium into a 300 micron thick silicon substrate. As you
well know typical Lithium drifted silicon detectors are a few mm thick
however I am interested in evaluating the radiation hardness of thin
lithium drifted silicon detectors.

Unfortunately evaporation of Lithium is a messy and dangerous process
and I am not allowed to do it in my clean room.

If you are further interested please contact me directly for a more
detailed explanation on the project.

Cheers

James

--
Dr. James Paul Grant
Postdoctoral Research Associate
Microsystems Technology Group
76 Oakfield Avenue Room 205
School of Engineering
University of Glasgow
Glasgow
Scotland
G12 8LS

Telephone: +44(0)141 330 6690

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation
Addison Engineering