MEMSnet Home: MEMS-Talk: Etching BCB or UV Glue
Etching BCB or UV Glue
2010-11-22
Vijay Rajaraman
2010-11-23
Michael D Martin
Etching BCB or UV Glue
Vijay Rajaraman
2010-11-22
Hello,

Has anyone successfully etched (selective or blanket) 10 microns of
cured BCB (cyclotene) or UV glue, landing on either Si or Al, without
residues ?

In case of selective etching, the preferred masking material is photoresist.

Is there any good reference material on etching such thicker polymer layers?

Do let me know.

Many thanks,
Vijay
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review