A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: spin coater vacuum path
spin coater vacuum path
2010-12-09
Jia Yao
2010-12-09
Andrew Sarangan
2010-12-09
Jia Yao
2010-12-09
Brad Cantos
2010-12-09
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Morrison, Richard H., Jr.
2010-12-10
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Shay
2010-12-09
Andrew Sarangan
2010-12-10
David Grove
2010-12-09
ZijianCao
2010-12-09
Jia Yao
2010-12-10
Huy
2010-12-13
Jia Yao
2010-12-14
Paul Grasso
spin coater vacuum path
Jia Yao
2010-12-09
Hi all,

I am having problem with spin coater. At first there were some photoresist
going into the chuck all the way to the bottom so the program stopped
automatically after a couple of seconds of running. Also the platform was
very hard to rotate by hand. After I cleaned the pathway which has the
photoresist, the platform moves freely but the vaccum is showing
insufficient value. Is there something blocking the vacuum
somewhere? How could I possibly check the block?

Thank you very much!

Jia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing