MEMSnet Home: MEMS-Talk: spin coater vacuum path
spin coater vacuum path
2010-12-09
Jia Yao
2010-12-09
Andrew Sarangan
2010-12-09
Jia Yao
2010-12-09
Brad Cantos
2010-12-09
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Morrison, Richard H., Jr.
2010-12-10
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Shay
2010-12-09
Andrew Sarangan
2010-12-10
David Grove
2010-12-09
ZijianCao
2010-12-09
Jia Yao
2010-12-10
Huy
2010-12-13
Jia Yao
2010-12-14
Paul Grasso
spin coater vacuum path
Jia Yao
2010-12-10
I took the parts out in the pathway and cleaned them so it is less likely
that there is some blockage than leakage. Any good way to check the leakage?
And I confirmed that the external vacuum pump and the vacuum sensor on the
spin coater are all right.

Thank you.
Jia

On Thu, Dec 9, 2010 at 2:31 PM, Gary Hillman  wrote:

> Gentlemen, there are two factors possibly at work here.  One is that the
> vacuum passageway is blocked, the other is that it is leaking.
>
> Gary Hillman
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.