A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: spin coater vacuum path
spin coater vacuum path
2010-12-09
Jia Yao
2010-12-09
Andrew Sarangan
2010-12-09
Jia Yao
2010-12-09
Brad Cantos
2010-12-09
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Morrison, Richard H., Jr.
2010-12-10
Gary Hillman
2010-12-10
Jia Yao
2010-12-10
Shay
2010-12-09
Andrew Sarangan
2010-12-10
David Grove
2010-12-09
ZijianCao
2010-12-09
Jia Yao
2010-12-10
Huy
2010-12-13
Jia Yao
2010-12-14
Paul Grasso
spin coater vacuum path
Morrison, Richard H., Jr.
2010-12-10
Hi,

Did you make sure to replace any "O"-Rings or gaskets. Cleaning them is
tough it is better to replace them.

Rick Morrison


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Jia Yao
Sent: Thursday, December 09, 2010 10:17 PM
To: General MEMS discussion
Subject: Re: [mems-talk] spin coater vacuum path

I took the parts out in the pathway and cleaned them so it is less
likely
that there is some blockage than leakage. Any good way to check the
leakage?
And I confirmed that the external vacuum pump and the vacuum sensor on
the
spin coater are all right.

Thank you.
Jia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
MEMStaff Inc.
Nano-Master, Inc.