MEMSnet Home: MEMS-Talk: Adhesion problem during 7740 glass wafer wet etching process
Adhesion problem during 7740 glass wafer wet etching process
2010-12-13
Xin Yan
2010-12-13
Zijian Cao
2010-12-13
Shay Kaplan
2010-12-14
Xin Yan
2010-12-13
Andrew Sarangan
2010-12-13
Mikael Evander
2010-12-14
Xin Yan
2010-12-14
Mikael Evander
2010-12-15
Xin Yan
2010-12-14
Xin Yan
2010-12-16
Andrew Sarangan
2010-12-15
Ned Flanders
Adhesion problem during 7740 glass wafer wet etching process
Xin Yan
2010-12-14
the sputtering  is  for  lift off. I'm afraid the Cr could not stand for
enough time, So i do the wet etching before removing the photoresist.  what
about heat the substrate to 80degreeC during sputtering to suppress the
pinhole?

Thank you Mikael

On Tue, Dec 14, 2010 at 12:55 AM, Mikael Evander wrote:

> I'd guess pinholes, a dirty Cr-film or cracks in the photoresist. Do you
> do anything with it after sputtering the chromium? I've had problems in
> the past until I realized that we've incorporated a plasma cleaning step
> of the chromium before depositing the photoresist. It worked great for a
> while but then started to act like your film does. The reason in  my case
> was that someone had started using the plasma cleaner for bonding PDMS and
> that contaminated the film enough to make the photoresist peel and then
> the chromium was attacked and dissolved pretty fast.
>
> Also check that the photoresist isn't cracked or under severe stress from
> baking.
>
> /mikael

--
Yan Xin
-Pen-Tung Sah MEMS Research Center,
-Xiamen University, CHINA
XMU HOME:
http://memsc.xmu.edu.cn/mems_renchaiduiwu/XuYuan_Chen-Group/index_1.html
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
MEMStaff Inc.