MEMSnet Home: MEMS-Talk: PDMS fine structures
PDMS fine structures
2010-12-12
DEBASHIS MAJI
2010-12-13
Gareth Jenkins
2010-12-13
[email protected]
2010-12-14
Michael Cooke
2010-12-14
DEBASHIS MAJI
2010-12-14
Bill Moffat
2010-12-15
Tsoll Doiiu
2010-12-22
DEBASHIS MAJI
PDMS fine structures
Tsoll Doiiu
2010-12-15
I'm gonna suggest that you did not allow PDMS to cool down completely, and use
too high curing temperature for a long time. Usually I use 80C for 20-25 min in
an oven, and than put the sample on a surface with a temperature below room T
for like a 10 min - after that I do not have any tearing of PR
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.