Hi all,

i would need to evaporate 80nm of Au on a thin diamond layer.
Cr is tipically used as adhesion layer while evaporating Au on Silicon.

Is a Cr adhesion layer needed also to evaporate Au on diamond ?
In the case Cr will not adhere on diamond, which other adhesion layer
should be used ?

Best regards,
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation