I am working on Chemical Based Depositions of  thinfilms and trying to get
rid of voids and precipitates deposited on the seeded silicon substrate.
Can anyone suggest me few tips... I have tried annealing for better
charecterization of thinfilms. Is there any other process that i could try
to improve the charecterstics of the thinfilms.

Please post your suggestion. It will be of great help to me.

Thanx
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
University Wafer