I am having a problem patterning SU8 on alumina substrates on top of a
patterned gold film.

I have some polished alumina substrates (approx 250 microns thick) with a
thin film (~1 micron) gold pattern on the top surface.  I am trying to
pattern SU8-3005 (approx 4 microns thick) as an interlayer dielectric on top
of the gold.  The SU8 pattern includes openings that are all on top of gold
features.  Using our current process, where the edge of the opening is
adjacent to a larger field of metal, the pattern develops out nicely in
about 5-7 minutes.  Where the edge of the opening is adjacent to the edge of
the metal, the pattern doesn't develop properly, even with extra long
development times (>30 min).  This is most evident where (for example) a 50
micron square via is patterned in SU8 at the edge of a 200 micron wide Au
line such that 3 sides of the via have a large field of metal adjacent to
the edge of the via, while the 4th edge is on top of the gold but adjacent
to bare alumina.  Three sides develop out properly, but a significant amount
of SU8 is left in the pattern along the fourth side of the via.  This effect
is independent of pattern orientation.  Note that large features (>100
microns) develop properly using our current process; smaller vias (even as
large as 35 microns), don't develop out at all.

Has anybody else seen this effect?  Is the problem likely to be related to
exposure control, thermal management or something else?  Any help or clues
as to how to address it would be greatly appreciated.

Thanks,
Rob
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics