MEMSnet Home: MEMS-Talk: Sloped microchannel
Sloped microchannel
2011-02-28
Tsoll Doiiu
2011-02-28
Nabhiraj Yalagoud
2011-02-28
Dr. Holger Becker
2011-03-04
khan waseem
2011-02-28
Dietrich Lueerssen
2011-02-28
Nabhiraj Yalagoud
2011-02-28
Kevin Nichols
2011-02-28
Bill Moffat
2011-03-01
Kevin Nichols
2011-03-01
Shao Guocheng
2011-03-11
eowin rohan
Sloped microchannel
Nabhiraj Yalagoud
2011-02-28
Dear Dietrich,

when the spinner starts spinning, centrifugal forces take over and gravity
effect to keep the liquid with angel will not be possible. As the speed
increases, irrespective of angle of substrate, the coating will be very
uniform.

Nabhiraj


On Mon, Feb 28, 2011 at 7:07 PM, Dietrich Lueerssen <
[email protected]> wrote:

> Hi there,
>
> I have not tried this suggestion. However, it would seem to me that if you
> mounted the substrate at an angle to the axis of rotation of the spinner
> (rather than it being perpendicular), you might be able to achieve the
> difference in height of the photoresist. Now it would be up to you to try
> and achieve that in your spinner...
>
> Good luck,
> Dietrich
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation