MEMSnet Home: MEMS-Talk: PDMS mold peeling off process
PDMS mold peeling off process
2011-03-17
첸로
2011-03-17
righeira carnegie
2011-03-17
Xiaohui Lin
2011-03-17
Mikael Evander
2011-03-18
righeira carnegie
2011-03-22
Tsoll Doiiu
2011-03-22
[email protected]
2011-03-17
Barbara Cortese
PDMS mold peeling off process
첸로
2011-03-17
Dear all,

I am using photolithography and PDMS mold technique to get a PDMS mold.

I'm having some troubles when I peel off the PDMS mold from the SU-8 master.
Even a very careful handing I can not get a good PDMS mold. After peeling off,
the pattern on the PDMS mold is always broken.

The SU-8 master's smallest width is 10um. Is it feasible in theory?

Can anyone give me some suggestions?

Thank you in advance

Regards
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Addison Engineering
MEMS Technology Review