A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS mold peeling off process
PDMS mold peeling off process
2011-03-17
첸로
2011-03-17
righeira carnegie
2011-03-17
Xiaohui Lin
2011-03-17
Mikael Evander
2011-03-18
righeira carnegie
2011-03-22
Tsoll Doiiu
2011-03-22
[email protected]
2011-03-17
Barbara Cortese
PDMS mold peeling off process
Barbara Cortese
2011-03-17
Hi,

it may depend on how thick your PDMS is, the mixing ratio, and curing
temperature.

Can you provide more details?

Barbara

---------- Initial Header -----------

>From      : [email protected]
To          : "mems-talk" [email protected]
Cc          :
Date      : Thu, 17 Mar 2011 11:57:20 +0800 (CST)
Subject : [mems-talk] PDMS mold peeling off process

> Dear all,
>
> I am using photolithography and PDMS mold technique to get a PDMS mold.
>
> I'm having some troubles when I peel off the PDMS mold from the SU-8 master.
Even a very careful handing I can not get a good PDMS mold. After peeling off,
the pattern on the PDMS mold is always broken.
>
> The SU-8 master's smallest width is 10um. Is it feasible in theory?
>
> Can anyone give me some suggestions?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Mentor Graphics Corporation
Harrick Plasma, Inc.