A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS mold peeling off process
PDMS mold peeling off process
2011-03-17
첸로
2011-03-17
righeira carnegie
2011-03-17
Xiaohui Lin
2011-03-17
Mikael Evander
2011-03-18
righeira carnegie
2011-03-22
Tsoll Doiiu
2011-03-22
[email protected]
2011-03-17
Barbara Cortese
PDMS mold peeling off process
Mikael Evander
2011-03-17
I've peeled of patterns that were 20 um and very long so it should work.
What I did, because I was having similar problems to you, was to coat the
master in a thin Teflon layer and it then released beautifully. My master
was all glass though so that may be easier ...

/Mikael

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of 첸로
Sent: Wednesday, March 16, 2011 8:57 PM
To: mems-talk
Subject: [mems-talk] PDMS mold peeling off process

Dear all,

I am using photolithography and PDMS mold technique to get a PDMS mold.

I'm having some troubles when I peel off the PDMS mold from the SU-8
master. Even a very careful handing I can not get a good PDMS mold. After
peeling off, the pattern on the PDMS mold is always broken.

The SU-8 master's smallest width is 10um. Is it feasible in theory?

Can anyone give me some suggestions?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics