MEMSnet Home: MEMS-Talk: Etching of SiN
Etching of SiN
2011-03-24
kapil kumar jain
2011-03-24
antwi nimo
2011-03-24
Mark West
2011-03-24
Benjamin Gesemann
2011-03-25
ozgur celik
Etching of SiN
Mark West
2011-03-24
If you are referring to H3PO4, the standard method for etching SiN is to
maintain a boiling solution at a given temperature. This will also control
the concentration. Straight from the bottle, H3PO4 will boil at
approximately 155°C and provide for an etch rate of approx 45A/min.
Increasing the temperature (boil point) up to 180°C will increase
concentration and the etch rate to around 100A/min.

Special tanks with condensing collars and lids are available for the nitride
etch process that help maintain concentration by refluxing water vapors.
Special temperature controllers are also used that control the heaters and
water addition to ensure that the solution is always boiling at a specific
temperature.

-----Original Message-----
From: kapil kumar jain [mailto:[email protected]]
Sent: Wednesday, March 23, 2011 10:24 PM
To: [email protected]
Subject: [mems-talk] Etching of SiN

What is the optimum concentration of SiN etchant ? The thickness is of
the order of 1000 A.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing