Dear all,

I am using photolithography technique to make a su-8 pattern. The smallest
feature width is 10um.

The mask shape is a square which side length is 10um.

After developing the su-8 pattern sharp features are always lost. The square
turns to a circle due to the reflection and diffraction and some optical
phenomenon.

Does anybody have any ideas about how to solve this problem?

Please give me some suggestions... except OPC and PSM.

Thanks in advance.

Regards
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.