Aarthi,

That sounds like a very thick layer for seed. Have you tried hard
bake/descum in RIE O2 plasma before wet etch?

Regards,
Glenn

-----Original Message-----
From: Aarthi Lavanya Dhanapaul [mailto:[email protected]]
Sent: Monday, April 04, 2011 8:31 PM
To: [email protected]
Subject: [mems-talk] Silicon etch


I have been trying to remove a 1 micron thick Chromium seed layer using
commercially available chrome etchant. But I find the etching is not
uniform, even though there is agitation as well as heating been done. And my
structures on top of chromium ends up being messy.

Can any one suggest a better alternative or suggestions.

Thanks
Aarthi

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
The Branford Group