A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: run-in/run-out errors in alignment of photomasks
run-in/run-out errors in alignment of photomasks
2011-05-13
Wei Tang
2011-05-13
Edouard Duriau
2011-05-13
Wei Tang
2011-05-18
Brad Cantos
2011-05-18
Wei Tang
2011-05-19
Brad Cantos
2011-05-19
Wei Tang
run-in/run-out errors in alignment of photomasks
Brad Cantos
2011-05-18
Hi Wei,

The lenses won't be a problem with a contact aligner.  I had this same
experience many years ago with the MJB3, and switching to quartz masks helped
quite a bit.  Of course, it depends on how critical your alignment is, and how
much temperature variation your masks, wafers and cleanroom experience.  Another
possible cause is the pressure placed on the mask when the wafer is brought into
contact.  If the pressure is too high (check the specs), the mask could bow
considerably, causing this problem.

Brad
_________________________________

Brad Cantos
[email protected]
http://holage.com




On 13 May 2011, at 11:26 AM, Wei Tang wrote:

> Hi, Edouard
>
> Thanks for the reply and sharing your experience! By mentioning
> aberrations of the lenses, are you referring to a stepper? I am using
> a contact aligner (MJB3), will the lenses aberrations play a role
> here?
>
> Wei
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.