A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: TMAH doesn't attack some of (100) silicon wafers
TMAH doesn't attack some of (100) silicon wafers
2011-07-06
胡小东
2011-07-06
Andrea Mazzolari
2011-07-06
UDDIPTA CHATTERJEE
2011-07-06
Morrison, Richard H., Jr.
TMAH doesn't attack some of (100) silicon wafers
Andrea Mazzolari
2011-07-06
Hi,

What is the TMAH concentration and temperature ?

I had the same "problem" you described. This could be due to native oxide on
the silicon wafers.

Try to dip wafers for about 1 min in BHF.  It should solve. For me it worked.

Best regards,
Andrea

-----Messaggio originale-----
Da: [email protected]
[mailto:[email protected]] Per conto di ???
Inviato: Wednesday, July 06, 2011 11:31 AM
A: [email protected]
Oggetto: [mems-talk] TMAH doesn't attack some of (100) silicon wafers

Hi, all,

While etching  (100) silicon wafers,  most of wafers were etched normally.
But few of (100) silicon wafers of the same batch were not etched at the
initial time. It seems that the initial reaction just didn't take place.

Has anyone had this experience?

Thanks!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer