MEMSnet Home: MEMS-Talk: Ti etching and S1813 resist
Ti etching and S1813 resist
2011-07-12
Shane GUO
2011-07-12
Kirt Williams
2011-07-12
Michael Martin
2011-07-12
Shane GUO
2011-07-12
G. Puebla-Hellmann
2011-07-13
David Springer
2011-07-17
Yunda Wang
2011-07-14
Shane GUO
Ti etching and S1813 resist
Shane GUO
2011-07-14
Hi all,

I tried 48% H2SO4 at 60C to etch Ti for about 6mins. It seems to work. The S1813
resist still remains there. However, after I use Remover PG to clean S1813
resist, the patterned Ti electrodes become very hard to observe. The colour of
Ti left on the substrate is quite light and almost invisible. I am wondering if
my etching time is too long or Remover PG can clean up Ti at the same time when
it cleans the resist?

Thank you in advance.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
University Wafer