A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Cr wet etching
Cr wet etching
2011-07-19
Judith Linacero Blanco
2011-07-20
Ned Flanders
2011-07-20
Ned Flanders
2011-07-22
eowin rohan
2011-07-20
Salam Gabran
2011-07-22
Jaroslaw Syzdek
2011-07-22
Roger Shile
2011-07-22
[email protected]
Cr wet etching
eowin rohan
2011-07-22
Yes, it is that orange stuff, but it is ceric ammonium NITRATE.

I agree with Ned about etch rate.

The recipe we use is as follows:
20 g Ce(NH4)2 (NO3)6
3.5 mL CH3COOH
and adding H2O till 100 mL

Eowin.



________________________________
Från: Ned Flanders 
Till: General MEMS discussion 
Skickat: ons 20 juli 2011 3:40:45
Ämne: Re: [mems-talk] Cr wet etching

Correction: I meant ceric ammonium NITRIDE etchant. Which also
contains perchloric acid. That orange stuff, in other words.

m

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing