A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Si3N4 etching using H3PO4
Si3N4 etching using H3PO4
2011-07-27
jumril yunas
2011-07-27
Bill Moffat
2011-07-27
Andrea Mazzolari
2011-07-28
jumril yunas
2011-07-27
Kirt Williams
2011-07-27
[email protected]
2011-07-27
Bill Moffat
Si3N4 etching using H3PO4
Bill Moffat
2011-07-27
I like Avi's input more than mine.  I gave a quick answer and did not read 150
C.  Vacuum Vapor Prime protects against long harsh etches but I have not run
high temperature as well.  It may work if you want to test it, send wafers.
Bill Moffat

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Wednesday, July 27, 2011 9:57 AM
To: Bill Moffat; General MEMS discussion
Subject: Re: [mems-talk] Si3N4 etching using H3PO4

If possible try a hi temp oxidation of the nitride, pattern resist, quick boe
etch then etch th nitride.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
MEMS Technology Review
Harrick Plasma, Inc.