MEMSnet Home: MEMS-Talk: Recommend a negative resist
Recommend a negative resist
2011-08-05
Ned Flanders
2011-08-05
Kevin Nichols
2011-08-06
Ned Flanders
2011-08-06
Bill Moffat
2011-08-06
Kevin Nichols
2011-08-07
Ned Flanders
2011-08-06
Xiaohui Lin
2011-08-05
gau s
2011-08-05
gau s
Recommend a negative resist
gau s
2011-08-05
Also for 1 micron resolution, thick SU 8 resist will induce lot of stress in the
film. Hence use a very thin SU 8 film may be upto 2 microns thick.

________________________________
From: gau s 
To: "[email protected]" ; General MEMS discussion

Sent: Friday, August 5, 2011 10:24 AM
Subject: Re: [mems-talk] Recommend a negative resist


You can try using SU 8 2000.5 or 2002 and adjust you spin coat parameters in
order to get 1 micron thickness.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics