Hello there,

 We use TG25 ES RTU gold solution from Technic company for our newly established
gold solution bath. But the solution vaporizes very fast (the solution level
dropped down about 1 inch in a week). We check the tank and there seems no leak.
I was wondering if any of you folks have run to this problem.

Thank you,
Nahid