Khaled Mohamed Ramadan
Metal compatibility of SU 8
Khaled Mohamed Ramadan
2011-10-03
I tried Cr before and I got a good result.

On Sat, Oct 1, 2011 at 5:22 PM, gau s  wrote:

> Hi,
>
> Does anyone know the compatibility of SU 8 with different metals(Aluminum,
> Copper, Gold, Titanium, Silver, etc.). Which Metals will give a good
> adhesion when deposited on top of SU 8?
>
> Best Regards,
> Gauri
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review