MEMSnet Home: MEMS-Talk: Ma-N400 resist for lift-off
Ma-N400 resist for lift-off
2011-10-04
Shane GUO
2011-10-05
Matthieu Nannini, Dr.
2011-10-07
Shane GUO
Ma-N400 resist for lift-off
Matthieu Nannini, Dr.
2011-10-05
Did you do a SEM image of the cross section of your resist pattern to make sure
you have a re-entrant profile ?

Are you using evap or sputtering ?


-----------------------------------
Matthieu Nannini
McGill Nanotools Microfab
Manager
t: 514 398 3310
c: 514 758 3311
f: 514 398 8434
http://miam2.physics.mcgill.ca/
------------------------------------

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group