Recipe of Ar plasma etching gold
2011-10-12
Yingtao Tian
2011-10-12
Bill Moffat
2011-10-12
Matthieu Nannini, Dr.
2011-10-12
志修 梁
2011-10-12
Yingtao Tian
2011-10-13
Kirt Williams
2011-10-30
Khaled Mohamed Ramadan
2011-10-31
Kirt Williams
Recipe of Ar plasma etching gold
Yingtao Tian
2011-10-12
Hi,

Thank you guys for replying. Actually, when I asked 'etching', I did mean the
plasma sputter off material. Because I have other components on some area of the
wafer, the wet etching process can damage my components. So, I am thinking an
inert Ar plasma may be better choice to remove the 100nm Au and Cr.

If any of you could give me something to start with, then I may be able to work
out my own parameters more quickly.

Thanks again.

Yingtao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.
Nano-Master, Inc.