A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: e-beam evaporation of gold
e-beam evaporation of gold
2011-12-05
Shane GUO
2011-12-06
Ruiz, Marcos Daniel (SGNCOE)
2011-12-06
Shane GUO
2011-12-06
Ruiz, Marcos Daniel (SGNCOE)
2011-12-07
Michael Martin
2011-12-06
Shane GUO
e-beam evaporation of gold
Shane GUO
2011-12-06
Hi Marcos,

Thanks for your prompt reply.

I have to change the typo in my last few sentences. My question is if the
problem is caused by a too thin gold layer or the lacking of adhesion layer?

I will try to add an adhesion layer to see how it changes the yield.


Thanks


>________________________________
> From: "Ruiz, Marcos Daniel (SGNCOE)" 
>To: Shane GUO ; General MEMS discussion 
>Sent: Monday, December 5, 2011 7:19:40 PM
>Subject: RE: [mems-talk] e-beam evaporation of gold
>
>The missing adhesion layer is your most likely culprit.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation