A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Optical absorbing material
Optical absorbing material
2012-01-05
Mike Whitson
2012-01-06
Glenn Silveira
2012-01-07
Alasdair Rankin
2012-01-05
Dean Hopkins
2012-01-06
Mike Whitson
2012-01-07
Shay
2012-01-06
Marc Reinig
2012-01-07
Dean Hopkins
Optical absorbing material
Marc Reinig
2012-01-06
Isn't Si fairly transparent above 1.5 microns?

Marco
==============================================
Marc Reinig                           Phone: (831) 459-4362
Laboratory for Adaptive Optics        Fax:   (831) 459-5717
UCO/Lick Observatory                  Email: [email protected]
University of California, Santa Cruz
1156 High Street
Santa Cruz, CA 95064


> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]] On Behalf
> Of Dean Hopkins
> Sent: Thursday, January 05, 2012 11:43 AM
> To: [email protected]
> Subject: Re: [mems-talk] Optical absorbing material
>
> Hi Mike, would you consider "Black Silicon"?
>
> Anyone with a deep RIE system can treat your wafers to form a black
silicon
> 'grass' on horizontal exposed silicon surfaces. The black silicon process
is
> frequently used  in tuning the process for best vertical sidewalls.
>
> * High broadband optical absorption.
> I don't know the spectral range of absorption, but it is really black,
black,
> black.
>
> * Spin coatable.
> No, but is that a performance requirement or an artifact of the existing
> process sequence?
>
> *
>  Electrical resistivity as high as possible. As etched the 'grass' is
conductive,
> but a thin oxide or nitride layer can passivate it.
>
> *
>  Patternable.
> Simple. Only open the areas you want to blacken to the RIE.
>
> * Long life.
> As long lived as the silicon in the rest of the device.
>
> I think I might be able to intercede with a fab to get samples run, if you
are
> interested.
>
> Best,
>
> Dean Hopkins
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics