Hi,

I have a structure covered in 100 nm SiO2 which I need to selectively
remove with BOE (using SU8 as a mask).  Beneath the SiO2 there will be
25 - 50 Angstroms of metal.  Any recommendations for which metal to use?
I was thinking Au or Cr, but haven't found any references for whether
and/or how quickly these metals etch in BOE/HF.

Thanks,
Jonathan

--
Jonathan J. Sapan 
Graduate Student Researcher
Center for Magnetic Recording Research
University of California at San Diego
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Harrick Plasma, Inc.
Nano-Master, Inc.