Kipp Schoenwald
2012-03-06
I am interested in using a metal as an etch stop for a dry etch of Silicon
Nitride, and I am looking for the following:

     1)  Can a metal be used as an etch stop for dry etching of PECVD
Si3N4; if so, which metals?
     2)  Does PECVD Si3N4 on metal adhere, grow, hermetically seal, and
stay structurally sound under bending load?

Supporting literature is very much appreciated!

Additional Process Details
  1) LPCVD Si3N4
  2) A metal
  3) PECVD Si3N4
  4) ICP Etch of PECVD layer down to the metal


Thank you in advance for your help,
Kipp Scheonwald
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing