Xiaohui Lin
2012-03-07
Kipp Schoenwald
2012-03-07
Xiaohui Lin
week adhesion of SU8 to glass or quartz
Xiaohui Lin
2012-03-07
So HDMS+SU8 or HDMS+omnicoat+SU8?

did you bake the HDMS before SU8 spinning?

On Wed, Mar 7, 2012 at 2:00 PM, Kipp Schoenwald
wrote:

> HMDS has worked for me on both Pyrex and Quartz.  I suspect it should work
> on glass just as well.
>
> Kipp
>
> On Tue, Mar 6, 2012 at 4:37 PM, Xiaohui Lin  >wrote:
>
> > hi all:
> >
> >    Could any one suggest how to improve the adhesion of SU8 2005 to glass
> > or quartz?
> >
> >     I tried glass+omnicoat+SU8, it is week. I also tried
> > quartz+omnicoat+SU8 , but still peel off when I put in plating solution
> > (pH=5).
> >
> >    Will HMDS work? or other adhesion promoter?
> >
> > thanks
> > _______________________________________________
> > Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> > provider of MEMS and Nanotechnology design and fabrication services.
> > Visit us at http://www.mems-exchange.org
> >
> > Want to advertise to this community?  See http://www.memsnet.org
> >
> > To unsubscribe:
> > http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> >
>
>
>
> --
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>



--
Lin, Xiaohui
Ph.D. Program in Electrical and Computer Engineering
Nanophotonics and Optical Interconnects Group
Microelectronics Research Center
The University of Texas at Austin
E-mail: [email protected]
Office: (512) 471-4349
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMStaff Inc.