Gary Hillman
2012-03-13
Fahad,  inorganic compounds do not have such a low melting point AND are
insulators.  I don't think nature likes that.  Gary
Gary Hillman
S-Cubed
PO Box 365
9 Mars Ct.
Montville, NJ 07045
phone 973-263-0640 ex 35
fax 973-263-8888
Check out our web site and Twitter at www.s-cubed.com


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Sk Fahad Chowdhury
Sent: Friday, March 09, 2012 6:30 PM
To: General MEMS discussion
Subject: [mems-talk] Spin on dielectric with low Tg


Hi,

I am looking for some spin on dielectric which needs to be inorganic
(preferably) and the glass transition temperature needs to be less than 180
deg C or as low as possible. Honestly speaking, I have almost no knowledge
about spin on dielectric. Good reference & vendor will be appreciated.

Thanks

Fahad
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 9.0.927 / Virus Database: 271.1.1/4268 - Release Date: 03/13/12
03:34:00

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer
Nano-Master, Inc.